Compressive strength, surface roughness, and surface microhardness of principle tricalcium silicate-based endodontic cements after universal adhesive application

dc.contributor.authorOlcay, K.
dc.contributor.authorGüneşer, Mehmet Burak
dc.contributor.authorDinçer, Asiye Nur
dc.contributor.authorUyan, Hatice Miray
dc.date.accessioned2022-04-01T07:12:42Z
dc.date.available2022-04-01T07:12:42Z
dc.date.issued2022
dc.departmentİstanbul Medipol Üniversitesi, Diş Hekimliği Fakültesi, Endodonti Ana Bilim Dalı
dc.description.abstractAims and Background: It was aimed to evaluate compressive strength (CS), surface roughness, and microhardness of mineral trioxide aggregate (ProRoot MTA) and Biodentine (BD) after adhesive application. Materials and Methods: Tests was carried out according to international ISO standard. ProRoot MTA and BD were prepared in Teflon molds according to manufacturer's instructions: n = 210 for CS; n = 210 for microhardness. Samples were incubated for 7 days at 37°C in 100% humidity. Surfaces were smoothed with up to 2000 grits of silicon-carbide sandpaper on abrasive device at 150 rpm, randomly divided into seven groups (n = 15). Clearfil Universal Bond, All Bond Universal, and Single Bond Universal (SBU) were applied in both total-etch and self-etch (SE) modes. Adhesives were applied according to manufacturers' recommendations (no adhesive used in control). CS was performed at speed of 1 mm/min, microhardness at 100 gr for 15 s. The surface roughness of the samples was analyzed with atomic force microscopy. Two-way analysis of variance and post hoc Tukey tests were used for the evaluation of the data. Results: Man CS and microhardness values between ProRoot MTA and BD were as follows: 24.9 N, 72.6 HV; 59.8 N, 59.0 HV, respectively. In CS, BD was higher than ProRoot MTA (P < 0.05). In other comparisons except for SBU SE group (P < 0.05), BD and ProRoot MTA showed similar results (P > 0.05). However, ProRoot MTA was found higher than BD regarding microhardness (P < 0.05). As a result of the adhesive application in both BD and ProRoot MTA groups, a decrease in surface roughness was observed compared to the control group. Conclusion: BD exhibited better results than ProRoot MTA regarding CS. However, ProRoot MTA was found to be more successful than BD in terms of microhardness. BD and ProRoot MTA showed similar physical properties in terms of surface roughness. To improve regenerative procedures, besides the selection of bioceramic cements, the interaction between cements and materials applied during coronal restoration should be considered.
dc.identifier.citationOlcay, K., Güneşer, M. B., Dinçer, A. N. ve Uyan, H. M. (2022). Compressive strength, surface roughness, and surface microhardness of principle tricalcium silicate-based endodontic cements after universal adhesive application. Nigerian Journal of Clinical Practice, 25(3), 231-238. https://doi.org/10.4103/njcp.njcp_1287_21
dc.identifier.doi10.4103/njcp.njcp_1287_21
dc.identifier.endpage238
dc.identifier.issn1119-3077
dc.identifier.issue3
dc.identifier.pmid35295042
dc.identifier.scopus2-s2.0-85126654748
dc.identifier.scopusqualityQ3
dc.identifier.startpage231
dc.identifier.urihttps://doi.org/10.4103/njcp.njcp_1287_21
dc.identifier.urihttps://hdl.handle.net/20.500.12511/9192
dc.identifier.volume25
dc.identifier.wos000884847100003en_US
dc.identifier.wosqualityQ4
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.indekslendigikaynakPubMed
dc.institutionauthorUyan, Hatice Miray
dc.language.isoen
dc.publisherNLM (Medline)
dc.relation.ispartofNigerian Journal of Clinical Practiceen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsAttribution-NonCommercial-ShareAlike 4.0 International*
dc.rightsinfo:eu-repo/semantics/openAccess
dc.rights.urihttps://creativecommons.org/licenses/by-nc-sa/4.0/*
dc.subjectBiodentine
dc.subjectCompressive Strength
dc.subjectMineral Trioxide Aggregate
dc.subjectRegenerative Endodontics
dc.subjectSurface Microhardness
dc.subjectSurface Roughness
dc.subjectTricalcium Silicate-Based Cement
dc.titleCompressive strength, surface roughness, and surface microhardness of principle tricalcium silicate-based endodontic cements after universal adhesive application
dc.typeArticle

Dosyalar

Orijinal paket
Listeleniyor 1 - 1 / 1
Yükleniyor...
Küçük Resim
İsim:
Uyan-Hatice-2022.pdf
Boyut:
1.55 MB
Biçim:
Adobe Portable Document Format
Açıklama:
Tam Metin / Full Text
Lisans paketi
Listeleniyor 1 - 1 / 1
Küçük Resim Yok
İsim:
license.txt
Boyut:
1.44 KB
Biçim:
Item-specific license agreed upon to submission
Açıklama: