dc.contributor.author | Yavuz, Tevfik | |
dc.contributor.author | Özyılmaz, Özgün Yusuf | |
dc.contributor.author | Öztürk, Atiye Nilgun | |
dc.contributor.author | Aykent, Filiz | |
dc.date.accessioned | 10.07.201910:49:13 | |
dc.date.accessioned | 2019-07-10T20:02:05Z | |
dc.date.available | 10.07.201910:49:13 | |
dc.date.available | 2019-07-10T20:02:05Z | |
dc.date.issued | 2016 | en_US |
dc.identifier.citation | Yavuz, T., Özyılmaz, Ö. Y., Öztürk, A. N. ve Aykent, F. (2016). Bond strength of resin composite to light activated bleached enamel. Nigerian Journal of Clinical Practice, 19(6), 766-771. https://dx.doi.org/10.4103/1119-3077.178909 | en_US |
dc.identifier.issn | 1119-3077 | |
dc.identifier.uri | https://dx.doi.org/10.4103/1119-3077.178909 | |
dc.identifier.uri | https://hdl.handle.net/20.500.12511/3543 | |
dc.description | WOS: 000391532500014 | en_US |
dc.description | PubMed ID: 27811449 | en_US |
dc.description.abstract | Objectives: This study evaluated the microtensile bond strength (mu TBS) of a resin composite bonded to bleached enamel as a function of bleaching conditions. Materials and Methods: The whiteness hydrogen peroxide (HP) bleaching agent containing 35% HP was applied to the central incisors' facial enamel surface and irradiated as follows: No treatment (G1; control); no light (G2); light-emitting diode, the 40s (G3); diode laser, the 20s (G4); and neodymium: yttrium aluminum garnet laser, 20s (G5). A Variolink II resin composite structure was then built up incrementally on the surface. The teeth were sectioned into three 1.2 mm x 1.2 mm wide "I"-shaped sections. The specimens were then subjected to microtensile testing at a crosshead speed of 1 mm/min. Data were analyzed using one-way ANOVA (alpha = 0.05) followed by the Tukey Honestly Significant Difference post-hoc test. The fractured surfaces were observed with a stereomicroscope at x 100 magnification. Results: One-way ANOVA revealed no statistical differences among the groups (P > 0.05). No differences appeared between the groups bonded 14 days after bleaching (P > 0.05). Mean mu TBS values (MPa) were as follows: 22.05 +/- 5.01 (G1); 19.6 +/- 5.6 (G2); 19.3 +/- 5.4 (G3); 20.08 +/- 2.08 (G4); and 18.1 +/- 4.8 (G5). Many adhesive failures occurred at the bleached and irradiated enamel surfaces. Conclusion: The various irradiation treatments following the application of the whiteness HP bleaching agent to enamel did not significantly reduce the mu TBS within a 14-day period. | en_US |
dc.language.iso | eng | en_US |
dc.publisher | Wolters Kluwer Medknow Publications | en_US |
dc.rights | info:eu-repo/semantics/openAccess | en_US |
dc.rights | Attribution-NonCommercial-ShareAlike 3.0 Unported | * |
dc.rights.uri | https://creativecommons.org/licenses/by-nc-sa/3.0/ | * |
dc.subject | Bleaching Agents | en_US |
dc.subject | Lasers | en_US |
dc.subject | Lasers Neodymium: Yttrium Aluminum Garnet | en_US |
dc.subject | Resin Bonding | en_US |
dc.subject | Tooth Bleaching | en_US |
dc.title | Bond strength of resin composite to light activated bleached enamel | en_US |
dc.type | article | en_US |
dc.relation.ispartof | Nigerian Journal of Clinical Practice | en_US |
dc.department | İstanbul Medipol Üniversitesi, Diş Hekimliği Fakültesi, Protetik Diş Tedavisi Ana Bilim Dalı | en_US |
dc.identifier.volume | 19 | en_US |
dc.identifier.issue | 6 | en_US |
dc.identifier.startpage | 766 | en_US |
dc.identifier.endpage | 771 | en_US |
dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | en_US |
dc.identifier.doi | 10.4103/1119-3077.178909 | en_US |
dc.identifier.wosquality | Q4 | en_US |
dc.identifier.scopusquality | Q3 | en_US |