dc.identifier.citationDilber, E., Yavuz, T., Kara, H. B. ve Öztürk, A. N.(2012).Comparison of the effects of surface treatments on roughness of two ceramic systems. Photomedicine and Laser Surgery, 30(6), 308-314. https://dx.doi.org/10.1089/pho.2011.3153en_US
dc.identifier.issn1549-5418
dc.identifier.issn1557-8550
dc.identifier.urihttps://dx.doi.org/10.1089/pho.2011.3153
dc.identifier.urihttps://hdl.handle.net/20.500.12511/3670
dc.descriptionWOS: 000305284500003en_US
dc.descriptionPubMed ID: 22506513en_US
dc.description.abstractObjective: The aim of this study was to evaluate the effects of different surface treatments on the surface roughness of lithium disilicate-based core (IPS Empress 2, shade 210, Ivoclar Vivadent, Schaan, Liechtenstein) and feldspathic ceramics (Vita VM9, VITA Zahnfabrik H. Rauter GmbH & Co. KG, Bad Sackingen, Germany). Background data: Er:YAG laser irradiation is expected to be an alternative surface treatment, thus enhances surface roughness of procelains and produces morphological changes. Methods: Fifty lithium disilicate-based core ceramic discs and 50 feldspathic ceramic discs were prepared (diameter, 10 mm; thickness, 1 mm) according to the manufacturers' instructions. All-ceramic discs were polished to standardize, and surface roughness of the discs was evaluated before treatment and serving as controls. Both of two ceramic groups were divided into five groups (n = 10), and the following treatments were applied: (1) sandblasting with aluminum oxide (Al2O3; Group SB); (2) Al2O3 + Er:YAG laser (Group SB-L); (3) Er:YAG laser irradiation (distance, 1 mm; 500 mJ; 20 Hz; 10W; manually, contact handpiece [R 14]) (Group L); (4) 5% hydrofluoric acid etching (Group HF); and (5) Er: YAG laser + 5% hydrofluoric acid (Group HF-L). Surface roughness was evaluated by profilometry, and specimens were then examined with atomic force microscopy. Results: Data were analyzed by Wilcoxon signed rank, Mann-Whitney U, and Kruskal-Wallis tests (alpha = 0.05). The Wilcoxon signed rank test results indicated that surface roughness after sandblasting was significantly different from the surface roughness after laser irradiation and acid etching (p < 0.001). Mann-Whitney U and Kruskal-Wallis test results indicated that groups SB and SB-L had significantly higher mean roughness values (p < 0.05) than those in the other groups. Conclusions: Groups SB and SB-L had rougher surfaces than the groups subjected to the other surface treatment methods. There was no significant difference in surface roughness between the HF acid etching, Er:YAG laser irradiation, and HF and Er:YAG (p < 0.05).en_US
dc.language.isoengen_US
dc.publisherMary Ann Liebert, Inc.en_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.subjectDental Acid Etchingen_US
dc.subjectEpidemiologyen_US
dc.subjectMaterials Testingen_US
dc.subjectCeramic Systemsen_US
dc.subjectSurface Treatmentsen_US
dc.titleComparison of the effects of surface treatments on roughness of two ceramic systemsen_US
dc.typearticleen_US
dc.relation.ispartofPhotomedicine and Laser Surgeryen_US
dc.departmentİstanbul Medipol Üniversitesi, Diş Hekimliği Fakültesi, Protetik Diş Tedavisi Ana Bilim Dalıen_US
dc.authorid0000-0002-9292-2074en_US
dc.identifier.volume30en_US
dc.identifier.issue6en_US
dc.identifier.startpage308en_US
dc.identifier.endpage314en_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.identifier.doi10.1089/pho.2011.3153en_US
dc.identifier.wosqualityQ2en_US
dc.identifier.scopusqualityQ2en_US


Bu öğenin dosyaları:

Thumbnail

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster