dc.contributor.authorYavuz, Tevfik
dc.contributor.authorÖzyılmaz, Özgün Yusuf
dc.contributor.authorÖztürk, Atiye Nilgun
dc.contributor.authorAykent, Filiz
dc.date.accessioned10.07.201910:49:13
dc.date.accessioned2019-07-10T20:02:05Z
dc.date.available10.07.201910:49:13
dc.date.available2019-07-10T20:02:05Z
dc.date.issued2016en_US
dc.identifier.citationYavuz, T., Özyılmaz, Ö. Y., Öztürk, A. N. ve Aykent, F. (2016). Bond strength of resin composite to light activated bleached enamel. Nigerian Journal of Clinical Practice, 19(6), 766-771. https://dx.doi.org/10.4103/1119-3077.178909en_US
dc.identifier.issn1119-3077
dc.identifier.urihttps://dx.doi.org/10.4103/1119-3077.178909
dc.identifier.urihttps://hdl.handle.net/20.500.12511/3543
dc.descriptionWOS: 000391532500014en_US
dc.descriptionPubMed ID: 27811449en_US
dc.description.abstractObjectives: This study evaluated the microtensile bond strength (mu TBS) of a resin composite bonded to bleached enamel as a function of bleaching conditions. Materials and Methods: The whiteness hydrogen peroxide (HP) bleaching agent containing 35% HP was applied to the central incisors' facial enamel surface and irradiated as follows: No treatment (G1; control); no light (G2); light-emitting diode, the 40s (G3); diode laser, the 20s (G4); and neodymium: yttrium aluminum garnet laser, 20s (G5). A Variolink II resin composite structure was then built up incrementally on the surface. The teeth were sectioned into three 1.2 mm x 1.2 mm wide "I"-shaped sections. The specimens were then subjected to microtensile testing at a crosshead speed of 1 mm/min. Data were analyzed using one-way ANOVA (alpha = 0.05) followed by the Tukey Honestly Significant Difference post-hoc test. The fractured surfaces were observed with a stereomicroscope at x 100 magnification. Results: One-way ANOVA revealed no statistical differences among the groups (P > 0.05). No differences appeared between the groups bonded 14 days after bleaching (P > 0.05). Mean mu TBS values (MPa) were as follows: 22.05 +/- 5.01 (G1); 19.6 +/- 5.6 (G2); 19.3 +/- 5.4 (G3); 20.08 +/- 2.08 (G4); and 18.1 +/- 4.8 (G5). Many adhesive failures occurred at the bleached and irradiated enamel surfaces. Conclusion: The various irradiation treatments following the application of the whiteness HP bleaching agent to enamel did not significantly reduce the mu TBS within a 14-day period.en_US
dc.language.isoengen_US
dc.publisherWolters Kluwer Medknow Publicationsen_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.rightsAttribution-NonCommercial-ShareAlike 3.0 Unported*
dc.rights.urihttps://creativecommons.org/licenses/by-nc-sa/3.0/*
dc.subjectBleaching Agentsen_US
dc.subjectLasersen_US
dc.subjectLasers Neodymium: Yttrium Aluminum Garneten_US
dc.subjectResin Bondingen_US
dc.subjectTooth Bleachingen_US
dc.titleBond strength of resin composite to light activated bleached enamelen_US
dc.typearticleen_US
dc.relation.ispartofNigerian Journal of Clinical Practiceen_US
dc.departmentİstanbul Medipol Üniversitesi, Diş Hekimliği Fakültesi, Protetik Diş Tedavisi Ana Bilim Dalıen_US
dc.identifier.volume19en_US
dc.identifier.issue6en_US
dc.identifier.startpage766en_US
dc.identifier.endpage771en_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.identifier.doi10.4103/1119-3077.178909en_US
dc.identifier.wosqualityQ4en_US
dc.identifier.scopusqualityQ3en_US


Bu öğenin dosyaları:

Thumbnail

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster

info:eu-repo/semantics/openAccess
Aksi belirtilmediği sürece bu öğenin lisansı: info:eu-repo/semantics/openAccess